USRE35660EExpiredUtility

Anti-chewing and anti-cribbing composition

Assignee: DYCO ASSOCIATES INCPriority: Jun 10, 1991Filed: Mar 21, 1995Granted: Nov 11, 1997
Est. expiryJun 10, 2011(expired)· nominal 20-yr term from priority
C09D 5/00A01N 25/24A01N 61/02
27
PatentIndex Score
1
Cited by
15
References
1
Claims

Abstract

A coating composition to prevent cribbing by a horse includes a solvent, a carrier, a non volatile chemical and a pigment .Iadd.if required.Iaddend.. The solvent comprises a combination of a higher aromatic solvent having a boiling point above 170° Centigrade . .(380° Fahrenheit).!., and crystals thereof combined with a carrier therefor. Further, non-volatile chemicals which would assist in penetration of a wood surface and in enhancing residual properties of the composition can be added to the base combination.

Claims

exact text as granted — not AI-modified
What is claimed and sought to be protected by Letters Patent of the United States is: . .1. A method for preventing chewing of wood by applying coating, having an odor objectionable to a horse, to a wood surface, wherein said method comprises the steps of: 
     
        about 10 millimeters of mercury..!.. .12.  The coating composition of claim 11, wherein: a. said aromatic solvent has molecular weight of about 150 to about 166;   b. said aromatic solvent has a boiling range above about 180° Centrigrade; and   c. said aromatic solvent has a vapor pressure of about 1.6 millimeters to about 8 millimeters of mercury..!.. .13. The coating composition of claim 12, wherein:   a. said aromatic solvent includes aromatic hydrocarbons having from 9 to 16 carbon atoms; and   b. said aromatic solvent contains primarily aromatic hydrocarbons having from 10 to 12 carbon atoms..!.. .14. The coating composition of claim 6, wherein said composition is applied to a wood surface by at least one device selected from the group consisting of a brush device, a roller device, a spraying device, or a dip tank device..!.. .15. The coating composition of claim 6, wherein said aromatic solvent includes a t least one liquid having 10 to 12 carbon atoms..!.. .16. The coating composition of claim 6, wherein:   a. said aromatic solvent has a molecular weight of about 140 to about 170;   b. said aromatic solvent has a boiling range above about 170° Centigrade; and   c. said aromatic solvent has a vapor pressure of about 1.4 millimeters to about 10 millimeters of mercury..!.. .17. The coating composition of claim 16, wherein:   a. said aromatic solvent has a molecular weight of about 150 to about 166;   b. said aromatic solvent has a boiling range above about 180° Centigrade; and   c. said aromatic solvent has a vapor pressure of about 1.6 millimeters to   
     
     
        about 8 millimeters of mercury..!..Iadd.18.  A method for preventing chewing of wood by applying coating, having an odor objectionable to a horse, to a wood surface, wherein said method comprises the steps of: (a) gathering ingredients for said coating consisting of (1) an aromatic solvent of 120-200 molecular weight having a boiling point range of 160°-293° C., a flash point range of 50°-105° C., a vapor pressure of below 4 millimeters of mercury at 38° C., crystals of said aromatic solvent, (2) a liquid carrier from the group consisting of an alkali refined soy bean oil and linseed oil, (3) a pigment, and (4) a non-volatile component carrier and binder from the group consisting of hydrocarbon resin, maleic resin and phenolic resin;   (b) blending said aromatic solvent and crystals if the crystals are not firmly within the aromatic solvent to form a homogeneous mixture;   (c) adding carrier, pigment and non-volatile component carrier and binder to said homogeneous mixture to form a coating, wherein the aromatic is 20-70% carrier 5-40% and the non-volatile component carrier and binder 5-40% of the coating by weight; and   (d) applying the coating to a wood surface in a quantity sufficient to   
     
     
        deter the horse from chewing said wood surface. .Iaddend..Iadd.19.  The method of claim 18, wherein said aromatic solvent is Aromatic 200. .Iaddend..Iadd.20. The method of claim 18, wherein said aromatic solvent is Aromatic 100. .Iaddend..Iadd.21. The method of claim 18, wherein said aromatic solvent includes aromatic hydrocarbons having from 8 to 16 carbon atoms and said aromatic solvent contains primarily aromatic hydrocarbons having from 10 to 12 carbon atoms. .Iaddend..Iadd.22. The method of claim 21, wherein: (a) said pigment is selected from the group consisting of carbon black, titanium dioxide, Quinacridone Red and Phthalocyanine Blue;   (b) said aromatic solvent being present at the range of 30 to 60 percent by weight, said non-volatile component carrier and binder being present at the range of 15 to 30 percent by weight, said carrier being present at the range of 15 to 30 percent by weight, and said pigment being present at the range of 15 to 30 percent by weight; and   (c) the step of applying the coating is accomplished by at least one device selected from a group consisting of a brush device, a roller device, a   
     
     
        spraying device, or a dip tank device. .Iaddend..Iadd.23.  A horse repellent coating composition which has an odor objectionable to a horse and prevents the chewing of wood by the horse, consisting of: (a) 20-70% by weight of an aromatic solvent of 120-200 molecular weight having a boiling point range of 160°-293° C., a flash point range of 50°-105° C., a vapor pressure of below 4 millimeters of mercury at 38° C. and crystals of said aromatic solvent;   (b) 5-40% by weight of a liquid carrier selected from the group consisting of an alkali refined soy bean oil and linseed oil:   (c) 5-40% by weight of a pigment; and   (d) 5-40% by weight of a non-volatile component carrier and binder from the group consisting of hydrocarbon resin, maleic resin and phenolic resin. .Iaddend..Iadd.24. The coating composition of claim 23, wherein said aromatic solvent is present at the range of 25-65% by weight, said non-volatile component carrier and binder is present at the range of 10-35%, said liquid carrier is present at the range of 10-35% by weight, and said pigment is present at the range of 10-35% by weight. .Iaddend..Iadd.25. The coating composition of claim 23, wherein said aromatic solvent is present at the range of 30-60% by weight, said non-volatile component carrier and binder is present at the range of 15-30% by weight, said liquid carrier is present at the range of 15-30% by weight, and said pigment is present at the range of 15-30% by weight.   
     
     
        .Iaddend..Iadd.26.  The coating composition of claim 23, wherein said aromatic solvent includes aromatic hydrocarbons having from 8 to 16 carbon atoms and said aromatic solvent contains primarily aromatic hydrocarbons having from 10 to 12 carbon atoms. .Iaddend..Iadd.27. The coating composition of claim 23, wherein said pigment is selected from the group consisting of carbon black, titanium dioxide, Quinacridone Red and Phthalocyanine Blue. .Iaddend..Iadd.28. The coating composition of claim 23, wherein: a. said aromatic solvent includes aromatic hydrocarbons having from 9 to 16 carbon atoms; and   b. said aromatic solvent contains primarily aromatic hydrocarbons having   
     
     
        from 10 to 12 carbon atoms. .Iaddend..Iadd.29.  The coating composition of claim 23, wherein said composition is applied to a wood surface by at least one device selected from the group consisting of a brush device, a roller device, a spraying device, or a dip tank device. .Iaddend..Iadd.30. The coating composition of claim 23, wherein said aromatic solvent includes at least one liquid having 10 to 12 carbon atoms. 
     
     
        .Iaddend..Iadd. 1.  A method for preventing chewing of wood by applying coating, having an odor objectionable to a horse, to a wood surface, wherein said method comprises the steps of: (a) gathering ingredients for said coating consisting of (1) an aromatic solvent of 120-200 molecular weight having a boiling point range of 160°-293° C., a flash point range of 50°-105° C., a vapor pressure of below 4 millimeters of mercury at 20° C., crystals of said aromatic solvent, (2) a liquid carrier from the group consisting of an alkali refined soy bean oil and linseed oil, and (3) a non-volatile component carrier and binder from the group consisting of hydrocarbon resin, maleic resin and phenolic resin;   (b) blending said aromatic solvent and crystals if the crystals are not firmly within the aromatic solvent to form a homogeneous mixture;   (c) adding carrier, non-volatile component carrier and binder to said homogeneous mixture to form a coating, wherein the aromatic is 20-70% carrier 5-40% and the non-volatile component carrier and binder 5-40% of the coating by weight; and   (d) applying the coating to a wood surface in a quantity sufficient to deter the horse from chewing said wood surface. .Iaddend..Iadd.32. The method of claim 31, wherein a pigment is added to the homogeneous mixture. .Iaddend..Iadd.33. The method of claim 31, wherein said aromatic solvent is Aromatic 200. .Iaddend..Iadd.34. The method of claim 31, wherein said aromatic solvent is Aromatic 100. .Iaddend..Iadd.35. The method of claim 31, wherein said aromatic solvent includes aromatic hydrocarbons having from 8 to 16 carbon atoms and said aromatic solvent contains primarily aromatic hydrocarbons having from 10 to 12 carbon atoms. .Iaddend..Iadd.36. The method of claim 32, wherein:   (a) said pigment is selected from the group consisting of carbon black, titanium dioxide, Quinacridone Red and Phthalocyanine Blue;   (b) said aromatic solvent being present at the range of 30 to 60 percent by weight, said non-volatile component carrier and binder being present at the range of 15 to 30 percent by weight, said carrier being present at the range of 15 to 30 percent by weight, and said pigment being present at the range of 15 to 30 percent by weight; and   (c) the step of applying the coating is accomplished by at least one device selected from a group consisting of a brush device, a roller device, a   
     
     
        spraying device, or a dip tank device. .Iaddend..Iadd.37.  A horse repellent coating composition which has an odor objectionable to a horse and prevents the chewing of wood by the horse, consisting of: (a) 20-70% by weight of an aromatic solvent of 120-200 molecular weight having a boiling point range of 160°-293° C., a flash point range of 50°-105° C., a vapor pressure of below 4 millimeters of mercury at 20° C., and crystals of said aromatic solvent;   (b) 5-40% by weight of a liquid carrier selected from the group consisting of an alkali refined soy bean oil and linseed oil; and   (c) 5-40% by weight of a non-volatile component carrier and binder from the group consisting of hydrocarbon resin, maleic resin and phenolic resin.   
     
     
        .Iaddend..Iadd.38.  The coating composition of claim 37, wherein said aromatic solvent includes aromatic hydrocarbons having from 8 to 16 carbon atoms and said aromatic solvent contains primarily aromatic hydrocarbons having from 10 to 12 carbon atoms. .Iaddend..Iadd.39. The coating composition of claim 37, wherein: a. said aromatic solvent includes aromatic hydrocarbons having from 9 to 16 carbon atoms; and   b. said aromatic solvent contains primarily aromatic hydrocarbons having   
     
     
        from 10 to 12 carbon atoms. .Iaddend..Iadd.40.  The coating composition of claim 37, wherein said composition is applied to a wood surface by at least one device selected from the group consisting of a brush device, a roller device, a spraying device, or a dip tank device. .Iaddend..Iadd.41. The coating composition of claim 37, wherein said aromatic solvent includes at least one liquid having 10 to 12 carbon atoms. .Iaddend.

Join the waitlist — get patent alerts

Track USRE35660E — get alerts on status changes and closely related new filings.

We store only your email — no account needed. See our privacy policy.