Method of aluminizing the inside of the panel of a television picture tube

Priority: Oct 25, 1974Filed: Feb 25, 1980Granted: Jun 9, 1981
Est. expiryOct 25, 1994(expired)· nominal 20-yr term from priority
H01J 9/20
4
PatentIndex Score
1
Cited by
15
References
1
Claims

Abstract

The invention relates to a method of aluminizing the inside of the panel of a television picture tube. When aluminizing the inside of the panel, blisters caused by the vaporizing lacquer, are likely to develop in the layer of aluminum, especially on the side walls of the panel portion. When taking care in accordance with the invention, that the coat of lacquer is roughened prior to the performance of the aluminizing process, these blisters are avoided.

Claims

exact text as granted — not AI-modified
What is claimed is:  .[.1. In a method of aluminizing the inside of the panel of a television picture tube wherein a lacquer forms an intermediate layer between the layer of fluorescent material and the layer of aluminum as applied thereafter by way of evaporation, the steps of applying the coat of lacquer drying said coat of lacquer and roughening said coat of lacquer onto the layer of fluorescent material, at least within the area of the lateral surfaces of the panel sufficiently to prevent the formation of blisters in the subsequently applied layer of aluminum caused by vaporization of said coat of lacquer when subsequently heated..]. .[.2. A method according to claim 1, wherein said roughening step is accomplished by is boric acid is sprayed onto the coat of lacquer, and dried..]. .[.3. A method according to claim 1, wherein said roughening step is accomplished by supplying a further coat of lacquer onto said first coat of lacquer..]. .[.4. The method according to claim 1, wherein said roughening step is accomplished by spraying ammonium carbonate in a aqueous solution into said coat of lacquer and thereafter drying said ammonium carbonate solution..]. .[.5. A method according to claim 1, wherein said roughening step is accomplished by roughening the side walls of said panel prior to the application of said coat of lacquer..]. .[.6. A method according to claim 5, wherein said roughening step is accomplished by sandbasting the side walls of said panel prior to the application of said coat of lacquer..]..Iadd. 7. In a method of aluminizing the inside of the panel of a television picture tube wherein a lacquer forms an intermediate layer between the layer of fluorescent material and the layer of aluminum as applied thereafter by way of evaporation, the steps of applying the coat of lacquer onto the layer of fluorescent material and onto the lateral surfaces of the panel not covered by fluorescent material, drying said coat of lacquer, spraying boric acid onto said coat of lacquer and drying said boric acid, thereby roughening said coat of lacquer on the layer of fluorescent material and within the area of the lateral surfaces of the panel sufficiently to prevent the formation of blisters in the subsequently applied layer of aluminum caused by vaporization of said coat of lacquer when subsequently heated. .Iaddend.