Described is a process and system for direct printing of a decorative pattern onto an extruded PVC slat. The process includes providing a hot extruded PVC slat; directly contacting a surface of the hot extruded PVC slat with a direct printing cylinder as the slat is moved in a downstream direction, where the cylinder has a pattern with a cell structure that receives ink and rotates to directly apply the ink in the form of the pattern onto the surface of the hot extruded PVC slat. The process also includes controlling a temperature of the direct printing cylinder to inhibit drying of the ink while present on the direct printing cylinder.

Claims

exact text as granted — not AI-modified
What is claimed is: 
     
         1 . A process for direct printing of a decorative pattern onto an extruded PVC slat, comprising:
 providing a hot extruded PVC slat;   directly contacting a surface of the hot extruded PVC slat with a direct printing cylinder as the slat is moved in a downstream direction, the cylinder comprising a pattern with a cell structure that receives ink and rotates to directly apply the ink in the form of the pattern onto the surface of the hot extruded PVC slat; and   controlling a temperature of the direct printing cylinder to inhibit drying of the ink while present on the direct printing cylinder.   
     
     
         2 . The process of  claim 1 , wherein controlling a temperature of the direct printing cylinder comprises cooling of the direct printing cylinder, wherein the cooling comprises feeding a cooling fluid into a bore within the cylinder to remove heat therefrom and producing a heated cooling fluid. 
     
     
         3 . The process of  claim 2 , wherein the heated cooling fluid is withdrawn from the direct printing cylinder and is cooled in order to regenerate the cooling fluid for recirculation back into the direct printing cylinder. 
     
     
         4 . The process of  claim 3 , wherein the cooling fluid is cooled to a temperature below 80° F. before cooling the direct printing cylinder. 
     
     
         5 . The process of  claim 2 , wherein the cooling fluid is cooled to a temperature between 50° F. and 60° F. before cooling the direct printing cylinder. 
     
     
         6 . The process of  claim 1 , further comprising measuring a temperature of the direct printing cylinder and/or of the extruded PVC slat and based on the measured temperature controlling the cooling of the direct printing cylinder. 
     
     
         7 . The process of  claim 1 , wherein multiple direct printing cylinders are arranged in series along a first side of the extruded PVC slat in order to provide multiple direct printed patterns thereon. 
     
     
         8 . The process of  claim 1 , wherein at least one additional direct printing cylinder is provided on an opposed side of the extruded PVC slat to provide a directly printed pattern onto the opposed side thereof. 
     
     
         9 . The process of  claim 1 , wherein the hot extruded PVC slat is at a temperature between 300° F. and 375° F. while contacting the direct printing cylinder. 
     
     
         10 . The process of  claim 4 , wherein the hot extruded PVC slat is at a temperature between 310° F. and 370° F. while contacting the direct printing cylinder. 
     
     
         11 . The process of  claim 5 , wherein the hot extruded PVC slat is at a temperature between 320° F. and 365° F. while contacting the direct printing cylinder. 
     
     
         12 . The process of  claim 1 , further comprising applying the ink onto the direct printing cylinder by passing the direct printing cylinder into an ink pan and then scraping off excess ink using a doctor blade. 
     
     
         13 . The process of  claim 1 , wherein a plurality of printing stations is provided, each printing station comprising one of the direct printing cylinder that directly prints onto the hot extruded PVC slat, and wherein each printing station is spaced apart from an adjacent printing station to allow ink applied at the previous printing station to dry prior to the subsequent printing station, and wherein each printing station is at least 24 inches away from the previous printing station. 
     
     
         14 . The process of  claim 1 , further comprising texturizing the printed PVC slat, and wherein the texturizing is performed while the printed PVC slat is at a temperature of 200° F. to 250° F. 
     
     
         15 . The process of  claim 1 , wherein after applying the ink into the PVC slat, the printed PVC slat is subjected to drying. 
     
     
         16 . The process of  claim 15 , wherein the drying comprising directing air at the PVC slats provided via high velocity air nozzle dryers that are provided within a hood that is heated. 
     
     
         17 . The process of  claim 16 , further comprising curing the printed PVC slats to produce a slat product and cutting the slat product to produce louvers for horizontal or vertical applications. 
     
     
         18 . A process for direct printing of a decorative pattern onto an extruded polymer slat, comprising:
 providing a hot extruded slat;   directly contacting a surface of the hot extruded slat with a direct printing cylinder as the slat is moved in a downstream direction and while the hot extruded slat is at a temperature between 320° F. and 365° F., the cylinder comprising a pattern with a cell structure that receives ink and rotates to directly apply the ink in the form of the pattern onto the surface of the hot extruded slat; and   contacting the direct printing cylinder with a cooling fluid to maintain a temperature of the direct printing cylinder to inhibit drying of the ink while present on the direct printing cylinder; and   subjecting the hot extruded slat to curing to cure the ink and produce a printed slat product.   
     
     
         19 . The process of  claim 18 , wherein the printed slat product is between 2 inches and 5 inches wide and 0.018 inches and 0.045 inches thick, and comprises a polyvinyl chloride (PVC) core with a printed surface that comprises cured ink provided in a decorative pattern. 
     
     
         20 . A system for direct printing of a decorative pattern onto an extruded PVC slat, comprising:
 a feed assembly for feeding PVC beads;   an extruder having an inlet for receiving the PVC beads from the feed assembly, a main section for melting the beads, and an outlet for extruding a hot PVC slat;   a printing station comprising
 a frame; 
 a direct printing cylinder mounted to the frame; 
 an ink supply assembly containing ink and configured such that the direct printing roller receives ink therefrom for direct application to the hot PVC slat; and 
 a cooling system coupled to the direct printing roller for removing heat from the same.