Abstract

A system ( 5 ) and method ( 800 ) for unit cell casting of titanium or titanium-alloys is disclosed herein. The system ( 5 ) comprises an external chamber ( 45 ), a crucible ( 10 ) positioned within the external chamber ( 45 ), an induction coil ( 15 ) positioned around the crucible, an internal chamber ( 40 ) positioned within the external chamber ( 45 ), and a mold ( 30 ) positioned within the internal chamber ( 40 ). The external chamber ( 45 ) is evacuated and a pressurized gas is injected into the evacuated external chamber ( 45 ) to create a pressurized external chamber ( 45 ). An ingot ( 20 ) is melted within the crucible utilizing induction heating generated by the induction coil ( 15 ). The internal chamber ( 40 ) is evacuated to create an evacuated internal chamber ( 40 ). The titanium alloy material of the ingot ( 20 ) is completely transferred into the mold ( 30 ) from the crucible ( 10 ) using a pressure differential created between the external chamber ( 45 ) and the internal chamber ( 40 ).

Claims

exact text as granted — not AI-modified
We claim as our invention the following: 
     
         1 . A method for unit cell casting of titanium or titanium-alloys, the method comprising:
 monitoring a pressure of an internal chamber utilizing a first vacuum gauge;   monitoring a pressure of an external chamber utilizing a second vacuum gauge;   transmitting the pressure of the internal chamber and the pressure of the external chamber to a programmable logic controller (PLC);   positioning a mold within the internal chamber;   evacuating an external chamber to create an evacuated external chamber wherein a ceramic crucible containing a titanium alloy ingot is positioned therein;   injecting a pressurized gas into the evacuated external chamber to create a pressurized external chamber with a pressure in excess of 1 atm;   melting the titanium alloy ingot within the ceramic crucible utilizing induction heating generated by an induction coil positioned around the ceramic crucible;   evacuating the internal chamber to create an evacuated internal chamber having a pressure no greater than 3×10 −2  atmosphere;   transferring the completely melted titanium alloy material into the mold from the crucible using a pressure differential created between the external chamber and the internal chamber;   wherein a minimal pressure differential is maintained between the external chamber and the internal chamber during the melting of the titanium alloy ingot;   wherein the pressure of the internal chamber and the pressure of the external chamber are monitored and communicated to the PLC during the casting process, and wherein the PLC controls the casting process based on the pressure of the internal chamber and the pressure of the external chamber.   
     
     
         2 . The method according to  claim 1  wherein the pressurized gas is argon. 
     
     
         3 . The method according to  claim 1  wherein a frequency generated in the induction coil ranges from 1 kilo-Hertz to 50 kilo-Hertz, and a power ranges from 15 kilo-Watts to 50 kilo-Watts. 
     
     
         4 . The method according to  claim 1  wherein an atmospheric pressure of the evacuated internal chamber ranges from 3×10 −2  atmosphere to 9.87×10 −13  atmosphere. 
     
     
         5 . The method according to  claim 1  wherein the mold is for a thin-walled golf club head. 
     
     
         6 . The method according to  claim 1  wherein the internal chamber is preheated at a temperature ranging from 1150° C. to 1250° C. 
     
     
         7 . The method according to  claim 1  wherein the PLC determines when to melt the titanium alloy based on the pressures of the internal chamber and the external chamber. 
     
     
         8 . The method according to  claim 7  wherein the PLC determines when to change the pressure of internal chamber and the external chamber. 
     
     
         9 . The method according to  claim 1  wherein an atmospheric pressure of the evacuated internal chamber ranges from 9.87×10 −7  atmosphere to 9.87×10 −13  atmosphere 
     
     
         10 . A system method for unit cell casting of titanium or titanium-alloys, the system comprising:
 an external chamber;   a ceramic crucible positioned within the external chamber;   an induction coil positioned around a bottom section of the ceramic crucible;   an internal chamber positioned within the external chamber; and   a mold positioned within the internal chamber;   a first vacuum gauge positioned within the internal chamber;   a second vacuum gauge positioned within the external chamber;   a PLC in communication with the first vacuum gauge, the second vacuum gauge, and the induction coil;   wherein a minimal pressure differential is maintained between the external chamber and the internal chamber during the melting of the titanium alloy ingot;   wherein the pressure of the internal chamber and the pressure of the external chamber are monitored and communicated to the PLC during the casting process, and wherein the PLC controls the casting process based on the pressure of the internal chamber and the pressure of the external chamber;   wherein the external chamber is evacuated to create an evacuated external chamber wherein the ceramic crucible contains a titanium alloy ingot positioned therein;   wherein a pressurized gas is injected into the evacuated external chamber to create a pressurized external chamber;   wherein the titanium alloy ingot is melted within the ceramic crucible utilizing induction heating generated by the induction coil positioned around the ceramic crucible;   wherein the internal chamber is evacuated to create an evacuated internal chamber;   wherein the titanium alloy material is completely transferred into the mold from the crucible using a minimal pressure differential created between the external chamber and the internal chamber.   
     
     
         11 . A method for unit cell casting of titanium or titanium-alloys, the method comprising:
 positioning a mold within an internal chamber of a casting chamber;   evacuating an external chamber to create an evacuated external chamber wherein a ceramic crucible containing a titanium alloy ingot is positioned therein;   injecting a pressurized gas into the evacuated external chamber to create a pressurized external chamber with a pressure in excess of 1 atmosphere;   melting the titanium alloy ingot within the ceramic crucible utilizing induction heating generated by an induction coil positioned around the ceramic crucible;   evacuating the internal chamber to create an evacuated internal chamber having a pressure no greater than 3×10 −2  atmosphere; and   utilizing a high pressure differential between the external chamber and the internal chamber to flow the completely melted titanium alloy material into the mold from the crucible.   
     
     
         12 . The method according to  claim 11  wherein the pressurized gas is argon. 
     
     
         13 . The method according to  claim 11  wherein a frequency generated in the induction coil ranges from 1 kilo-Hertz to 50 kilo-Hertz, and a power ranges from 15 kilo-Watts to 50 kilo-Watts. 
     
     
         14 . The method according to  claim 11  wherein an atmospheric pressure of the evacuated internal chamber ranges from 3×10 −2  atmosphere to 9.87×10 −7  atmosphere. 
     
     
         15 . The method according to  claim 11  wherein the mold is for a thin-walled golf club head. 
     
     
         16 . The method according to  claim 11  wherein the internal chamber is preheated at a temperature ranging from 1150° C. to 1250° C. 
     
     
         17 . The method according to  claim 11  wherein a PLC determines when to melt the titanium alloy based on the pressures of the internal chamber and the external chamber. 
     
     
         18 . The method according to  claim 7  wherein the PLC determines when to change the pressure of internal chamber and the external chamber. 
     
     
         19 . The method according to  claim 1  wherein an atmospheric pressure of the evacuated internal chamber ranges from 9.87×10 −7  atmosphere to 9.87×10 −13  atmosphere