Stucco-Based Surfacing System And Method
Abstract
A building surfacing system is described, the system including a stucco substrate affixed to and disposed upon a support panel, a primer coating applied to a surface of the stucco substrate so as to form a primed stucco substrate, a first sealant coating applied to the primed stucco substrate, an intermediate mesh layer disposed upon the first sealant coating, and a second sealant coating applied to the intermediate mesh layer while the intermediate mesh layer is disposed upon the first sealant coating. A related method for providing a water-proof exterior surface to a building structure is further described.
Claims
exact text as granted — not AI-modified1 . A building surfacing system, the system comprising:
a stucco substrate affixed to and disposed upon a support panel, a primer coating applied to a surface of the stucco substrate so as to form a primed stucco substrate, a first sealant coating applied to the primed stucco substrate, an intermediate mesh layer disposed upon the first sealant coating, and a second sealant coating applied to the intermediate mesh layer while the intermediate mesh layer is disposed upon the first sealant coating.
2 . The surfacing system according to claim 1 , wherein the first and second sealant coatings each comprise a ceramic-fortified acrylic polymer emulsion.
3 . The surfacing system according to claim 2 , further comprising at least one decorative coating applied to the second sealant coating.
4 . The surfacing system according to claim 1 , wherein the stucco substrate further comprising a metal lath disposed between the support panel and the stucco substrate.
5 . The surfacing system according to claim 4 , further comprising at least one decorative coating applied to the second sealant coating.
6 . The surfacing system according to claim 4 , wherein the intermediate mesh layer is comprised of a woven fabric.
7 . The surfacing system according to claim 4 , wherein the first and second sealant coatings each comprise a ceramic-fortified acrylic polymer emulsion.
8 . A method of providing an exterior surface to a building structure, the method comprising
applying a stucco substrate to a support panel, which support panel is affixed, or configured to be affixed, to the building structure, applying a primer coating to a surface of the stucco substrate so as to form a primed stucco substrate, applying a first sealant coating to the primed stucco substrate, disposing an intermediate mesh layer upon the applied first sealant coating, and applying a second sealant coating to the intermediate mesh layer disposed upon the applied first sealant coating,
so as to form the exterior surface of the building structure.
9 . The method according to claim 8 , wherein the first and second sealant coatings each comprise a ceramic-fortified acrylic polymer emulsion.
10 . The method according to claim 9 , further comprising applying at least one decorative coating to the second sealant coating.
11 . The method according to claim 8 , further comprising attaching a metal lath to the support panel and applying the stucco substrate to the metal lath when applying the stucco substrate to the support panel.
12 . The method according to claim 11 , further comprising at least one decorative coating applied to the second sealant coating.
13 . The method according to claim 11 , where the intermediate mesh layer comprised of a woven fabric.
14 . The method according to claim 11 , wherein the first and second sealant coatings each comprise a ceramic-fortified acrylic polymer emulsion.Join the waitlist — get patent alerts
Track US2017009459A1 — get alerts on status changes and closely related new filings.
We store only your email — no account needed. See our privacy policy.