A method for bonding stainless steel members includes: contacting a first stainless steel member with a second stainless steel member that has a strain exceeding 50% reduction; and heating the first and second stainless steel members to a re-crystallization initiation temperature or higher, after the contacting.
Claims
exact text as granted — not AI-modifiedWhat is claimed is:
1 . A method for bonding stainless steel members comprising:
contacting a first stainless steel member with a second stainless steel member that has a strain exceeding 50% reduction; and heating the first and second stainless steel members to a re-crystallization initiation temperature or higher, after the contacting.
2 . The method for bonding stainless steel members as claimed in claim 1 , wherein the first stainless steel member has a strain exceeding 50% reduction.
3 . The method for bonding stainless steel members as claimed in claim 1 , wherein in the heating, the first stainless steel member and the second stainless steel member are heated to a temperature that is equal to the re-crystallization initiation temperature or higher and is equal to the re-crystallization initiation temperature plus 100 degrees C. or lower.
4 . A stainless steel which is obtained by bonding the first stainless steel member and the second stainless steel member by the method for bonding stainless steel members as claimed in claim 1 .
5 . A method for bonding stainless steel members comprising:
contacting a first austenitic stainless steel member with a second austenitic stainless steel member that contains at least 30 volume % of martensite; and heating the first and second austenitic stainless steel members to an As temperature or higher, after the contacting.
6 . The method for bonding stainless steel members as claimed in claim 5 , wherein the first austenitic stainless steel member contains at least 30 volume % of martensite.
7 . The method for bonding stainless steel members as claimed in claim 5 , wherein in the heating, the first austenitic stainless steel member and the second austenitic stainless steel member are heated to a temperature that is equal to the As temperature or higher and is equal to a re-crystallization initiation temperature plus 100 degrees C. or lower.
8 . A stainless steel which is obtained by bonding the first austenitic stainless steel member and the second austenitic stainless steel member by the method for bonding stainless steel members as claimed in claim 5 .Join the waitlist — get patent alerts