Abstract

A process for producing geometric shaped catalyst bodies K whose active material is a multielement oxide of stoichiometry [Bi 1 W b O x ] a [Mo 12 Z 1 c Z 2 d Fe e Z 3 f Z 4 g Z 5 h O y ] 1 , in which a finely divided oxide Bi 1 W b O x with the particle size d 50 A1 and, formed from element sources, a finely divided intimate mixture of stoichiometry Mo 12 Z 1 c Z 2 d Fe e Z 3 f Z 4 g Z 5 h with the particle size d 90 A2 are mixed in a ratio of a:1, this mixture is used to form shaped bodies and these are treated thermally, where (d 50 A1 ) 0.7 ·(d 90 A2 ) 1.5 ·(a) −1 ≧820. A shaped catalyst body obtained by the process. A catalyst obtained by grinding the shaped catalyst body. A process for heterogeneously catalyzing the partial gas phase oxidation of an alkane, alkanol, alkanal and/or an alkenal of 3 to 6 carbon atoms using the catalyst.

Claims

exact text as granted — not AI-modified
1 . (canceled) 
     
     
         2 . A shaped catalyst body comprising, as an active material, a multielement oxide having stoichiometry (I):
   [Bi 1 W b O x ] a [Mo 12 Z 1   c Z 2   d Fe e Z 3   f Z 4   g Z 5   h O y ] 1   (I)
   wherein:   Z 1  is nickel, cobalt, or a mixture thereof;   Z 2  is an alkali metal, an alkaline earth metal, thallium, or any mixture thereof;   Z 3  is zinc, phosphorus, arsenic, boron, antimony, tin, cerium, vanadium, chromium, bismuth, or any mixture thereof;   Z 4  is silicon, aluminum, titanium, tungsten, zirconium, or any mixture thereof;   Z 5  is copper, silver, gold, yttrium, lanthanum, a lanthanide, or any mixture thereof;   a is 0.1 to 3;   b is 0.1 to 10;   c is 1 to 10;   d is 0.01 to 2;   e is 0.01 to 5;   f is 0 to 5;   g is 0 to 10;   h is 0 to 1; and   x and y are numbers determined by the valency and frequency of the elements in stoichiometry (I) other than oxygen,   
       wherein the shaped catalyst body is produced by a process comprising:
 (I) preforming a finely divided mixed oxide Bi 1 W b O x  having a particle diameter d 50   A1  reported in the length unit μm, as starting material A1, with the proviso that 1 μm≦d 50   A1 ≦10 μm; 
 (II) mixing sources of the elements other than oxygen in the component T=[Mo 12 Z 1   c Z 2   d Fe e Z 3   f Z 4   g Z 5   h O y ] 1  of the multielement oxide in an aqueous medium, to obtain an intimate aqueous mixture M, with the proviso that
 each of the sources employed, in the course of preparation of the aqueous mixture M, passes through a degree of division Q for which its diameter d 90   Q  is ≦5 μm, and 
 the aqueous mixture M comprises the elements Mo, Z 1 , Z 2 , Fe, Z 3 , Z 4 , and Z 5  in the stoichiometry (I*)
   Mo 12 Z 1   c Z 2   d Fe e Z 3   f Z 4   g Z 5   h   (I*);
 
 
 
 (III) drying and adjusting the degree of division d 90   A2  of the aqueous mixture M, to obtain a finely divided starting material A2 having a particle diameter d 90   A2  reported in the length unit μm, with the proviso that 200 μm≧d 90   A2 ≧20 μm; 
 (IV) mixing starting material A1 and starting material A2, or starting material A1, starting material A2 and finely divided shaping assistant, to form a finely divided starting material A3, with the proviso that the starting material A3 comprises the elements other than oxygen introduced into the starting material A3 via starting materials A1 and A2 in the multielement oxide I in the stoichiometry (I**):
   [Bi 1 W b ] a [Mo 12 Z 1   c Z 2   d Fe e Z 3   f Z 4   g Z 5   h ] 1   (I**);
 
 
 (V) forming a geometric shaped body V with the finely divided starting material A3; and 
 (VI) thermally treating the shaped body V at an elevated temperature, to obtain the shaped catalyst body, 
 wherein the value F of the product
   (d 50   A1 ) 0.7 ·(d 90   A2 ) 1.5 ·(a −1 )
 
 
 is ≧820. 
 
     
     
         3 . A catalyst obtained by grinding the shaped catalyst body of  claim 2 . 
     
     
         4 . A process for heterogeneously catalyzed partial gas phase oxidation of an alkane, alkanol, alkanal, alkene, alkenal, or any mixture thereof, which comprises from 3 to 6 carbon atoms over a catalyst bed, wherein the catalyst bed comprises the shaped catalyst body of  claim 2 . 
     
     
         5 . The process of  claim 4 , which is a process for heterogeneously catalyzed partial gas phase oxidation of propene to acrolein. 
     
     
         6 . The process of  claim 4 , which is a process for heterogeneously catalyzed partial gas phase oxidation of isobutene to methacrolein. 
     
     
         7 . The process of  claim 4 , which is a process for ammoxidation of propene to acrylonitrile or a process for ammoxidation of isobutene to methacrylonitrile.