B29C 49/0411B29C 49/22B29C 49/0005B32B 7/02B32B 7/027B29K 2105/26B29C 48/0017B65D 1/40Y10T428/1352B32B 27/36B32B 2250/02Y10T428/1393B32B 27/08B29K 2995/002B29K 2067/003B32B 2250/244B29C 48/022B32B 2272/00B29K 2995/0026B29C 48/09B29L 2031/7158B32B 2307/4026B32B 2250/40B32B 2250/04B29K 2105/0094B32B 2250/03B32B 2439/60B65D 1/0215B29C 48/21Y10T428/1397B32B 1/02B32B 1/00
56
PatentIndex Score
0
Cited by
0
References
0
Claims
Abstract
An extruded PET parison includes a first extruded polymer comprising PET, and a second extruded polymer comprising PET. In embodiments, the first extruded polymer and the second extruded polymer are co-extruded, and the first extruded polymer has an intrinsic viscosity that is higher that the intrinsic viscosity of the second extruded polymer. A monolayer embodiment is also disclosed. In embodiments, a monolayer extruded PET container is comprised of bottle grade PET resin that has been solid stated and may have an IV from about 0.96 to about 1.4.
Claims
exact text as granted — not AI-modifiedWhat is claimed is:
1 . An extruded PET parison comprising:
a first extruded polymer comprising PET; and a second extruded polymer comprising PET; wherein the first and second polymers are co-extruded, the first and second extruded polymers are in a solid state, and the first extruded polymer has an intrinsic viscosity that is higher that the intrinsic viscosity of the second extruded polymer.
2 . The parison of claim 1 , wherein the first extruded polymer has an intrinsic viscosity of at least 0.96.
3 . The parison of claim 1 , wherein the first extruded polymer has an intrinsic viscosity from about 1.0 to about 1.4.
4 . The parison of claim 1 , wherein the second extruded polymer has an intrinsic viscosity of less than 0.85.
5 . The parison of claim 1 , wherein the second extruded polymer has an intrinsic viscosity of about 0.80 to about 0.87.
6 . The parison of claim 1 , wherein the second extruded polymer comprises post-consumer recycled (PCR) PET or regrind PET.
7 . The parison of claim 1 , wherein the second extruded polymer includes a colorant.
8 . The parison of claim 1 , wherein the cross-sectional thickness of the first extruded polymer is at least about 0.20 of the total parison thickness.
9 . The parison of claim 1 , wherein the cross-sectional thickness of the second extruded polymer is less than about 0.80 of the total parison thickness.
10 . The parison of claim 1 , including one or more additional extruded polymer layers.
11 . The parison of claim 10 , wherein the one or more additional extruded polymer layers comprise recycled or reground material.
12 . A container formed from the parison of claim 1 .
13 . An extruded PET parison comprising:
an extruded monolayer polymer comprising PET; wherein the extruded monolayer polymer is in a solid state, and the extruded monolayer polymer has an intrinsic viscosity from about 0.96 to about 1.4 and is devoid of chain extenders.
14 . The parison of claim 13 , wherein the intrinsic viscosity is about 1.1.
15 . A container formed from the parison of claim 13 .
16 . The container of claim 15 , wherein the container is substantially free of striations and haze.Join the waitlist — get patent alerts
Track US2014134372A1 — get alerts on status changes and closely related new filings.
We store only your email — no account needed. See our privacy policy.