US2013252374A1PendingUtilityA1

Semiconductor packaging method and structure thereof

Assignee: CHIPBOND TECHNOLOGY CORPPriority: Feb 16, 2012Filed: May 14, 2013Published: Sep 26, 2013
Est. expiryFeb 16, 2032(~5.6 yrs left)· nominal 20-yr term from priority
H10W 74/15H10W 99/00H10W 72/074H10W 72/073H10W 72/261H10W 72/072H10W 72/241H10W 72/351H10W 72/353H10W 72/354H10W 72/352H10W 72/325H10W 90/724H10W 72/252H10W 90/734H10W 95/00H01L 21/50
45
PatentIndex Score
0
Cited by
0
References
0
Claims

Abstract

A semiconductor packaging method includes providing a substrate having a plurality of pads, each of the pads comprises a first coupling surface having a plurality of first conductive contact areas and a plurality of first non-conductive contact areas; forming a conductible gel with anti-dissociation function on the substrate, said conductible gel includes a plurality of conductive particles and a plurality of anti-dissociation substances; mounting a chip on the substrate, said chip comprises a plurality of copper-containing bumps, each of the copper-containing bumps comprises a ring surface and a second coupling surface having a plurality of second conductive contact areas and a plurality of second non-conductive contact areas, wherein the conductive particles are electrically connected with the first conductive contact areas and the second conductive contact areas, said anti-dissociation substances are in contact with the second non-conductive contact area, and the ring surfaces are covered with the anti-dissociation substances.

Claims

exact text as granted — not AI-modified
What is claimed is: 
     
         1 . A semiconductor packaging method at least comprising:
 providing a substrate having an upper surface and a plurality of pads disposed on the upper surface, wherein each of the pads comprises a first coupling surface having a plurality of first conductive contact areas and a plurality of first non-conductive contact areas;   forming a conductible gel with anti-dissociation function on the upper surface and the pads of the substrate, wherein the conductible gel with anti-dissociation function includes a plurality of conductive particles and a plurality of anti-dissociation substances; and   mounting a chip on the substrate, the chip comprises an active surface facing toward the upper surface of the substrate and a plurality of copper-containing bumps disposed at the active surface, wherein the conductible gel with anti-dissociation function covers the copper-containing bumps, each of the copper-containing bumps comprises a second coupling surface and a ring surface, said second coupling surface comprises a plurality of second conductive contact areas and a plurality of second non-conductive contact areas, said copper-containing bumps are electrically connected with the pads via the conductive particles located between the first coupling surfaces and the second coupling surfaces, said conductive particles are electrically connected with the first conductive contact areas of the first coupling surfaces and the second conductive contact areas of the second coupling surfaces, wherein the anti-dissociation substances are located between adjacent conductive particles, each of the first coupling surfaces and each of the second coupling surfaces, said anti-dissociation substances are in contact with the second non-conductive contact areas of the second coupling surfaces, and the ring surfaces of the copper-containing bumps are covered with the anti-dissociation substances.   
     
     
         2 . The semiconductor packaging method in accordance with  claim 1 , wherein the anti-dissociation substances are in contact with the first non-conductive contact areas of the first coupling surfaces. 
     
     
         3 . The semiconductor packaging method in accordance with  claim 1 , wherein each of the pads comprises a lateral surface being covered with the anti-dissociation substances. 
     
     
         4 . The semiconductor packaging method in accordance with  claim 1 , wherein the anti-dissociation substance can be an organic solderability preservative. 
     
     
         5 . The semiconductor packaging method in accordance with  claim 4 , wherein the material of the organic solderability preservative can be chosen from one of benzimidazole or imidazole derivative. 
     
     
         6 . The semiconductor packaging method in accordance with  claim 5 , wherein the imidazole derivative can be one of Brenzotriazole, Phenylimidazole, Substituted Benzimidazole, Aryl Phonylimidazole or a mixture thereof, and the benzimidazole can be one of Brenzotriazole, Phenylimidazole, Substituted Benzimidazole, Aryl Phonylimidazole or a mixture thereof. 
     
     
         7 . The semiconductor packaging method in accordance with  claim 1 , wherein the material of the copper-containing bumps can be chosen from one of copper/nickel or copper/nickel/gold.