US2012271270A1PendingUtilityA1

Plastic container comprising cyclic polyolefin layer

Assignee: OZAKI KAZUHIKOPriority: Nov 22, 2007Filed: Jun 29, 2012Published: Oct 25, 2012
Est. expiryNov 22, 2027(~1.3 yrs left)· nominal 20-yr term from priority
A61P 3/08A61P 3/10A61P 39/06A61P 25/28B32B 2307/7265B32B 2307/546B32B 2307/30B32B 2307/412A61K 9/0019B32B 2307/7242A61J 1/10B32B 2307/31B32B 2250/24A61K 31/4152Y10T428/2826B32B 27/32B32B 27/08B32B 2270/00B32B 27/325B32B 27/302B32B 2439/80A61P 1/04B32B 2307/308B32B 2307/558B32B 2307/51B32B 2307/50A61J 1/1468
42
PatentIndex Score
0
Cited by
0
References
0
Claims

Abstract

The present invention provides and a plastic container and multilayered films, which comprises a heat-sealable seal layer, a cyclic polyolefin layer, and an outermost layer, wherein the seal layer comprises polypropylene, the cyclic polyolefin layer comprises a cyclic polyolefin polymer or a cyclic polyolefin copolymer, and the outermost layer comprises a layer containing polypropylene, and which further comprises a resin composition layer comprises a blended product of a propylene polymer and a styrene elastomer. The plastic container of the present invention can suppresses a reduction in the medicament content of a liquid-state medicament and is excellent in terms of shock resistance, handling ability during the filling of the container with the medicament, and the moldability and transparency of the container.

Claims

exact text as granted — not AI-modified
1 - 18 . (canceled) 
     
     
         19 . A multilayered film, comprising a heat-sealable seal layer, a cyclic polyolefin layer, and an outermost layer, wherein the seal layer comprises polypropylene, the cyclic polyolefin layer comprises a cyclic polyolefin polymer or a cyclic polyolefin copolymer, and the outermost layer comprises a layer containing polypropylene, and said multilayered film further comprises a resin composition layer comprising a blended product of a propylene polymer and a styrene elastomer; provided that a five-layered plastic film composed of only a seal layer-an adhesive layer-a barrier layer-an adhesive layer-a material layer, wherein each of the seal layer and the material layer consists of only a polypropylene elastomer having a melting point of 165° C., each of the adhesive layers consists of only MODIC manufactured by Mitsubishi Chemical Corporation, and the barrier layer consists of only a cyclic polyolefin polymer having a glass transition temperature of 136° C., is excluded. 
     
     
         20 . A plastic container comprising:
 multilayered films each comprising a heat-sealable seal layer, a cyclic polyolefin layer, and an outermost layer, wherein the seal layer comprises polypropylene, the cyclic polyolefin layer comprises a cyclic polyolefin polymer or a cyclic polyolefin copolymer, and the outermost layer comprises a layer containing polypropylene; and   a resin composition layer comprising a blended product of a propylene polymer and a styrene elastomer, in a state in which the seal layers are laminated on each other such that they face each other;   wherein the plastic container is molded by heat sealing peripheral portions of the multilayered films; and   wherein the plastic container is filled with a solution comprising an active ingredient excluding a pyrazolone derivative represented by the formula (I), a physiologically acceptable salt thereof, a hydrate thereof, or a solvate thereof:   
       
         
           
           
               
               
           
         
         wherein R 1  represents a hydrogen atom, an aryl, an alkyl containing 1 to 5 carbon atoms, or an alkoxycarbonylalkyl containing 3 to 6 carbon atoms in total; R 2  represents a hydrogen atom, an aryloxy, an arylmercapto, an alkyl containing 1 to 5 carbon atoms, or a hydroxyalkyl containing 1 to 3 carbon atoms; or R 1  and R 2  together represent an alkylene containing 3 to 5 carbon atoms; R 3  represents a hydrogen atom, an alkyl containing 1 to 5 carbon atoms, a cycloalkyl containing 5 to 7 carbon atoms, a hydroxyalkyl containing 1 to 3 carbon atoms, a benzyl, naphthyl or phenyl, or a phenyl substituted with 1 to 3 identical or different substituents selected from the group consisting of an alkoxy containing 1 to 5 carbon atoms, a hydroxyalkyl containing 1 to 3 carbon atoms, an alkoxycarbonyl containing 2 to 5 carbon atoms in total, an alkylmercapto containing 1 to 3 carbon atoms, an alkylamino containing 1 to 4 carbon atoms, a dialkylamino containing 2 to 8 carbon atoms in total, a halogen atom, a trifluoromethyl, a carboxyl, a cyano, a hydroxyl group, a nitro, an amino, and an acetamide. 
       
     
     
         21 . The plastic container according to  claim 20 , further comprising a resin composition layer or a polyethylene layer on the surfaces of both sides of the cyclic polyolefin layer. 
     
     
         22 . The plastic container according to  claim 21 , which comprises a resin composition layer having a fusion peak temperature only in a temperature range from 120° C. or higher to 170° C. or lower and also having a heat of fusion from 5 J/g or more to 20 J/g or less on the surfaces of both sides of the cyclic polyolefin layer. 
     
     
         23 . The plastic container according to  claim 20 , wherein the cyclic polyolefin of the cyclic polyolefin layer is a ring-opening polymer hydrogenation product of dicyclopentadiene or a derivative thereof. 
     
     
         24 . The plastic container according to  claim 20 , wherein the cyclic polyolefin layer has a glass transition temperature (Tg) of 80° C. to 120° C. 
     
     
         25 . The plastic container according to  claim 20 , wherein the melt flow rate (230° C., 21.2 N) value of the cyclic polyolefin layer is 1 to 20 (g/10 minutes). 
     
     
         26 . The plastic container according to  claim 20 , wherein the melt flow rate (230° C., 21.2 N) value of the seal layer and/or the outermost layer is 1 to 4 (g/10 minutes). 
     
     
         27 . The plastic container according to  claim 20 , wherein the bending elasticity of the seal layer and/or the outermost layer is 400 to 600 MPa. 
     
     
         28 . The plastic container according to  claim 20 , wherein the maximum fusion peak temperature of the seal layer is 125° C. to 135° C. 
     
     
         29 . The plastic container according to  claim 20 , wherein the highest fusion peak temperature of the seal layer is 150° C. to 160° C. 
     
     
         30 . The plastic container according to  claim 20 , wherein the fusion peak temperature of the outermost layer is 160° C. to 170° C. 
     
     
         31 . The plastic container according to  claim 20 , wherein the plastic film has a tensile elasticity of 300 MPa or less. 
     
     
         32 . The plastic container according to  claim 20 , which can be sterilized at 115° C. for 30 minutes or more. 
     
     
         33 . The plastic container according to  claim 20 , which can be sterilized at 121° C. for 15 minutes or more. 
     
     
         34 . The plastic container according to  claim 20 , which is in the form of an infusion bag. 
     
     
         35 . The plastic container according to  claim 20 , which is placed together with an oxygen absorber into a poorly air-permeable container. 
     
     
         36 . A plastic container comprising:
 a heat-sealable seal layer, a cyclic polyolefin layer, and an outermost layer, wherein the seal layer comprises polypropylene, the cyclic polyolefin layer comprises a cyclic polyolefin polymer or a cyclic polyolefin copolymer, and the outermost layer comprises a layer containing polypropylene; and   a resin composition layer comprising a blended product of a propylene polymer and a styrene elastomer; but   
       excluding a five-layered plastic film composed only of a seal layer, an adhesive layer, a barrier layer, an adhesive layer and a material layer, wherein each of the seal layer and the material layer consists only of a polypropylene elastomer having a melting point of 165° C., each of the adhesive layers consists only of MODIC manufactured by Mitsubishi Chemical Corporation, and the barrier layer consists only of a cyclic polyolefin polymer having a glass transition temperature of 136° C.

Join the waitlist — get patent alerts

Track US2012271270A1 — get alerts on status changes and closely related new filings.

We store only your email — no account needed. See our privacy policy.