US2010163200A1PendingUtilityA1

Method for making readily defibered pulp product

Assignee: WEYERHAEUSER COPriority: Dec 31, 2008Filed: Dec 31, 2008Published: Jul 1, 2010
Est. expiryDec 31, 2028(~2.4 yrs left)· nominal 20-yr term from priority
D21H 17/63D21H 17/675
57
PatentIndex Score
0
Cited by
0
References
0
Claims

Abstract

A wet-laid wood pulp product containing cellulose pulp fibers and elongate precipitated calcium carbonate having a diameter of 0.015 to 0.6 microns at its maximum diameter and a length of 1 to 10 microns and the calcium carbonate being incorporated within the sheet and a method for making the product.

Claims

exact text as granted — not AI-modified
1 . A method of making a wet laid cellulose pulp sheet comprising
 providing cellulose pulp fibers to a headbox,   providing elongate precipitated calcium carbonate having a diameter of 0.015 to 0.6 microns at its maximum diameter and a length of 1 to 10 microns to the headbox.   forming a wet sheet comprising the cellulose pulp fibers and the elongate precipitated calcium carbonate,   dewatering and drying the sheet to form a wet-laid pulp sheet incorporating within the sheet the elongate nano or near nano precipitated calcium carbonate.   
   
   
       2 . The method of  claim 1  wherein the elongate precipitated calcium carbonate is present in the amount of 3 to 40% of the weight of the cellulose pulp. 
   
   
       3 . The method of  claim 1  wherein the elongate precipitated calcium carbonate is present in the amount of 3 to 15% of the weight of the cellulose pulp. 
   
   
       4 . The method of  claim 1  wherein the elongate precipitated calcium carbonate is 1 to 3 microns in length. 
   
   
       5 . The method of  claim 1  wherein the elongate precipitated calcium carbonate is 3 to 10 microns in length. 
   
   
       6 . The method of  claim 1  wherein the elongate precipitated calcium carbonate is 0.015 to 0.45 microns in diameter at its maximum diameter. 
   
   
       7 . The method of  claim 6  wherein the elongate precipitated calcium carbonate is present in the amount of 3 to 40% of the weight of the cellulose pulp. 
   
   
       8 . The method of  claim 6  wherein the elongate precipitated calcium carbonate is present in the amount of 3 to 15% of the weight of the cellulose pulp. 
   
   
       9 . The method of  claim 6  wherein the elongate precipitated calcium carbonate is 1 to 3 microns in length. 
   
   
       10 . The method of  claim 6  wherein the elongate precipitated calcium carbonate is 3 to 10 microns in length.

Join the waitlist — get patent alerts