US2010059164A1PendingUtilityA1

Methods and Kits for Application of Wood Flooring

Individually held — no corporate assignee on recordPriority: Sep 9, 2008Filed: Sep 9, 2009Published: Mar 11, 2010
Est. expirySep 9, 2028(~2.1 yrs left)· nominal 20-yr term from priority
E04F 13/10E04F 15/02E04F 21/20
50
PatentIndex Score
0
Cited by
0
References
0
Claims

Abstract

A kit is described which includes an acrylic composition comprising acrylic polymer in an amount of from about 8 weight percent to about 42 weight percent and an alkanolamine in an amount of from about 0.05 weight percent to about 0.5 weight percent. The kit also includes a trowel blade, the blade having an application edge defining a plurality of generally rectangular teeth, at least one of the teeth including an integrally connected projection extending from the bottom edge of the at least one tooth. The trowel blade is configured to spread the composition across a surface with the projection causing a portion of the surface to not receive the composition. The composition is configured to form an adhesive bond between the surface and wood flooring material with application of the wood flooring material causing the composition to spread across the portion of the surface that did not receive the composition.

Claims

exact text as granted — not AI-modified
1 . A method for applying an adhesive and sealer composition comprising:
 spreading a composition over a surface with a trowel, the composition comprising either a moisture-curing urethane composition or an acrylic composition, the moisture-curing urethane composition comprising petroleum distillate in an amount of from about 2 weight percent to about 12 weight percent and polymeric isocyanate in an amount of from about 0.1 weight percent to about 3 weight percent, the acrylic composition comprising acrylic polymer in an amount of from about 8 weight percent to about 42 weight percent and an alkanolamine in an amount of from about 0.05 weight percent to about 0.5 weight percent, the trowel comprising a blade having an application edge defining a plurality of generally rectangular teeth, at least one of the teeth including an integrally connected projection extending from the bottom edge of the at least one tooth, the trowel blade configured to spread the composition across the surface with the projection causing a portion of the surface to not receive the composition;   applying wood flooring material onto the composition, the composition configured to form an adhesive bond between the surface and the wood flooring material with application of the wood floor causing the composition to spread across the portion of the surface that did not receive the composition.   
     
     
         2 . The method of  claim 1 , wherein the moisture-curing urethane composition or the acrylic composition has a viscosity of from about 130,000 cps to about 160,000 cps. 
     
     
         3 . The method of  claim 1 , wherein the moisture-curing urethane composition or the acrylic composition has a viscosity of from about 140,000 cps to about 155,000 cps. 
     
     
         4 . The method of  claim 1 , wherein the moisture-curing urethane composition comprises petroleum distillate in an amount of from about 5 weight percent to about 10 weight percent. 
     
     
         5 . The method of  claim 1 , wherein the acrylic composition comprises alkanolamine in an amount of from about 0.1 weight percent to about 0.4 weight percent. 
     
     
         6 . The method of  claim 1 , wherein the moisture-curing urethane composition or the acrylic composition is configured to prevent moisture from the surface from contacting the wood flooring material. 
     
     
         7 . The method of  claim 1 , wherein the moisture-curing urethane composition or the acrylic composition is configured to act as a crack suppressant for the surface. 
     
     
         8 . The method of  claim 1 , wherein the moisture-curing urethane composition or the acrylic composition further comprises an anti-microbial component. 
     
     
         9 . A method for applying an adhesive and sealer composition comprising:
 spreading a composition over a surface with a trowel, the composition comprising a moisture-curing urethane composition, the moisture-curing urethane composition comprising petroleum distillate in an amount of from about 2 weight percent to about 12 weight percent and polymeric isocyanate in an amount of from about 0.1 weight percent to about 3 weight percent, the trowel comprising a blade having an application edge defining a plurality of generally rectangular teeth, at least one of the teeth including an integrally connected projection extending from the bottom edge of the at least one tooth, the trowel blade configured to spread the composition across the surface with the projection causing a portion of the surface to not receive the composition;   applying wood flooring material onto the composition, the composition configured to form an adhesive bond between the surface and the wood flooring material with application of the wood floor causing the composition to spread across the portion of the surface that did not receive the composition.   
     
     
         10 . A method for applying an adhesive and sealer composition comprising:
 spreading a composition over a surface with a trowel, the composition comprising an acrylic composition, the acrylic composition comprising acrylic polymer in an amount of from about 8 weight percent to about 42 weight percent and an alkanolamine in an amount of from about 0.05 weight percent to about 0.5 weight percent, the trowel comprising a blade having an application edge defining a plurality of generally rectangular teeth, at least one of the teeth including an integrally connected projection extending from the bottom edge of the at least one tooth, the trowel blade configured to spread the composition across the surface with the projection causing a portion of the surface to not receive the composition;   applying wood flooring material onto the composition, the composition configured to form an adhesive bond between the surface and the wood flooring material with application of the wood floor causing the composition to spread across the portion of the surface that did not receive the composition.   
     
     
         11 . A kit for applying an adhesive and sealer composition comprising:
 a moisture-curing urethane composition comprising petroleum distillate in an amount of from about 2 weight percent to about 12 weight percent and polymeric isocyanate in an amount of from about 0.1 weight percent to about 3 weight percent; and   a trowel blade, the blade having an application edge defining a plurality of generally rectangular teeth, at least one of the teeth including an integrally connected projection extending from the bottom edge of the at least one tooth, the trowel blade configured to spread the composition across a surface with the projection causing a portion of the surface to not receive the composition, the composition configured to form an adhesive bond between the surface and wood flooring material with application of the wood flooring material causing the composition to spread across the portion of the surface that did not receive the composition.   
     
     
         12 . The kit of  claim 11 , wherein the moisture-curing urethane composition has a viscosity of from about 130,000 cps to about 160,000 cps. 
     
     
         13 . The kit of  claim 11 , wherein the moisture-curing urethane composition has a viscosity of from about 140,000 cps to about 155,000 cps. 
     
     
         14 . The kit of  claim 11 , wherein the moisture-curing urethane composition comprises petroleum distillate in an amount of from about 5 weight percent to about 10 weight percent. 
     
     
         15 . The kit of  claim 11 , wherein the moisture-curing urethane composition is configured to prevent moisture from the surface from contacting the wood flooring material. 
     
     
         16 . A kit for applying an adhesive and sealer composition comprising:
 an acrylic composition comprising acrylic polymer in an amount of from about 8 weight percent to about 42 weight percent and an alkanolamine in an amount of from about 0.05 weight percent to about 0.5 weight percent; and   a trowel blade, the blade having an application edge defining a plurality of generally rectangular teeth, at least one of the teeth including an integrally connected projection extending from the bottom edge of the at least one tooth, the trowel blade configured to spread the composition across a surface with the projection causing a portion of the surface to not receive the composition, the composition configured to form an adhesive bond between the surface and wood flooring material with application of the wood flooring material causing the composition to spread across the portion of the surface that did not receive the composition.   
     
     
         17 . The kit of  claim 16 , wherein the acrylic composition has a viscosity of from about 130,000 cps to about 160,000 cps. 
     
     
         18 . The kit of  claim 16 , wherein the acrylic composition has a viscosity of from about 140,000 cps to about 155,000 cps. 
     
     
         19 . The kit of  claim 16 , wherein the acrylic composition comprises alkanolamine in an amount of from about 0.1 weight percent to about 0.4 weight percent. 
     
     
         20 . The kit of  claim 16 , wherein the acrylic composition is configured to prevent moisture from the surface from contacting the wood flooring material.

Join the waitlist — get patent alerts

Track US2010059164A1 — get alerts on status changes and closely related new filings.

We store only your email — no account needed. See our privacy policy.