US2009293676A1PendingUtilityA1

Method of recovering valuable metals from waste

Assignee: KOIZUMI TETSUYUKIPriority: Jun 2, 2008Filed: Aug 5, 2008Published: Dec 3, 2009
Est. expiryJun 2, 2028(~1.8 yrs left)· nominal 20-yr term from priority
C22B 7/001C22B 1/005H05K 3/22Y02P10/20H05K 1/0366H05K 2203/1105C22B 15/0056H05K 2203/178C22B 7/005C22B 11/025Y02P70/50
32
PatentIndex Score
0
Cited by
0
References
0
Claims

Abstract

A method which allows recovery of valuable metals in simple steps from printed wiring board or the like is provided. The waste is an integrated industrial waste containing a glass fiber, an epoxy resin and valuable metals such as copper, iron, gold and aluminum. The method comprises heating the industrial waste to a temperature at which the glass fiber does not melt but degrades, followed by removing the degraded glass fiber.

Claims

exact text as granted — not AI-modified
1 . A method of recovering valuable metals from waste, the waste being an integrated industrial waste containing a glass fiber, an epoxy resin and valuable metals such as copper, iron, gold and aluminum, comprising
 heating the industrial waste to a temperature at which the glass fiber does not melt but degrades,   removing the degraded glass fiber, and thus,   recovering the valuable metals contained in the waste.   
   
   
       2 . The method of recovering valuable metals from waste according to  claim 1 , wherein the temperature condition applied to the industrial wastes is in the range of 500° C. for 20 minute or more and 1000° C. for about 10 minutes. 
   
   
       3 . The method of recovering valuable metals from waste according to  claim 1 , wherein the temperature condition applied to the industrial wastes is in the range of 750° C. for 30 minute or more and 1000° C. for about 10 minutes.