Abstract

A process for treating hair fibers comprising: applying to the hair fibers at least one cosmetic composition comprising, in a cosmetically acceptable medium, at least one polysiloxane/polyurea block copolymer; and subsequently or simultaneously heating the hair fibers at a temperature ranging from 50 to 280° C.

Claims

exact text as granted — not AI-modified
1 . A process for treating hair fibers comprising:
 applying to the hair fibers at least one cosmetic composition comprising, in a cosmetically acceptable medium, at least one polysiloxane/polyurea block copolymer, and simultaneously or successively,   heating the hair fibers at a temperature ranging from 50 to 280° C.   
   
   
       2 . The process of  claim 1 , wherein the at least one copolymer is non-ionic. 
   
   
       3 . The process of  claim 1 , wherein the at least one copolymer comprises at least one polyurethane block. 
   
   
       4 . The process of  claim 1 , wherein the at least one copolymer comprises only polysiloxane blocks and polyurea blocks. 
   
   
       5 . The process of  claim 1 , wherein the at least one copolymer does not comprise a polyurethane block. 
   
   
       6 . The process of  claim 1 , wherein the polysiloxane block of the at least one copolymer is present in an amount, by weight, of polysiloxane greater than 5%, relative to the total weight of the copolymer. 
   
   
       7 . The process of  claim 6 , wherein the polysiloxane block of the at least one copolymer is present in an amount greater than 50% by weight, relative to the total weight of the copolymer. 
   
   
       8 . The process of  claim 7 , wherein the polysiloxane block of the at least one copolymer is present in an amount greater than 90% by weight, relative to the total weight of the copolymer. 
   
   
       9 . The process of  claim 1 , wherein the at least one polysiloxane/polyurea copolymer is chosen from those of formula (I): 
     
       
         
         
             
             
         
       
       wherein: 
       R is a monovalent hydrocarbon-based radical, optionally substituted by fluorine or chlorine, having 1 to 20 carbon atoms; 
       X is an alkylene radical having 1 to 20 carbon atoms, in which non-neighboring methylene units may be replaced by —O— radicals; 
       A is an oxygen atom or an —NR′— amino radical; 
       Z is an oxygen atom or an —NR′— amino radical; 
       R′ is hydrogen or an alkyl radical having 1 to 10 carbon atoms; 
       Y is a divalent hydrocarbon-based radical, where appropriate optionally substituted by fluorine or chlorine, having 1 to 20 carbon atoms; 
       D is an alkylene radical, optionally substituted by fluorine, chlorine, C 1 -C 6  alkyl or C 1 -C 6  alkyl ester, having 1 to 700 carbon atoms, wherein non-neighboring methylene units may be replaced by —O—, —COO—, —OCO— or —OCOO— radicals; 
       n is a number ranging from 1 to 4,000; 
       a is a number of at least 1; 
       b is a number ranging from 0 to 40; 
       c is a number ranging from 0 to 30; and 
       d is a number greater than 0, 
       on the condition that A is an —NH— radical in at least one of the (a) units. 
     
   
   
       10 . A process of  claim 1 , wherein the at least one copolymer is obtained by a process comprising:
 reacting a cyclic silazane of formulae (2) or (2′):   
     
       
         
         
             
             
         
       
       with an organic silicon compound of formula (3):
   (HO)(R 2 SiO) n-1 [H]  (3) 
 
       to give an aminoalkylpolydiorganosiloxane of formula (4):
   H 2 N—X—[SiR 2 O] n SiR 2 —X—NH 2   (4); 
 wherein the aminoalkylpolydiorganosiloxane of formula (4) is then polymerized with a diisocyanate of formula (5):
   OCN—Y—NCO  (5); and 
 
 
       further wherein 
       X is an alkylene radical having 1 to 20 carbon atoms, in which non-neighboring methylene units may be replaced by —O— radicals; 
       Y is a divalent hydrocarbon-based radical, where appropriate optionally substituted by fluorine or chlorine, having 1 to 20 carbon atoms; 
       R is a monovalent hydrocarbon-based radical, optionally substituted by fluorine or chlorine, having 1 to 20 carbon atoms; 
       and n is a number ranging from 1 to 4,000. 
     
   
   
       11 . A process of  claim 1 , wherein the at least one copolymer is polyureadimethicone. 
   
   
       12 . A process of  claim 1 , wherein the at least one polysiloxane/polyurea block copolymer is present in an amount ranging from 0.05 to 20%, relative to the weight of the composition. 
   
   
       13 . A process of  claim 1 , wherein the at least one polysiloxane/polyurea block copolymer is present in an amount ranging from 0.1 to 15% of the weight of the composition applied. 
   
   
       14 . A process of  claim 1 , wherein the at least one polysiloxane/polyurea block copolymer is present in an amount ranging from 0.5 to 10% of the weight of the composition applied. 
   
   
       15 . A process of  claim 1 , wherein the at least one composition further comprises at least one adjuvant chosen from organomodified silicones; cationic, non-ionic, anionic and amphoteric polymers; peptides and derivatives thereof; protein hydrolysates; waxes; swelling agents; penetrants; anionic, cationic, non-ionic, amphoteric and zwitterionic surfactants; agents for combating hair loss; anti-dandruff agents; natural and synthetic associative and non-associative thickeners; suspension agents; sequestering agents; sunscreens; vitamins and provitamins; fatty acids; fatty alcohols; mineral, plant and synthetic oils; fragrances and preservatives. 
   
   
       16 . A process of  claim 1 , wherein the at least one composition is applied to wet hair fibers. 
   
   
       17 . A process of  claim 1 , wherein the hair fibers are heated at a temperature ranging from 60 to 250° C. 
   
   
       18 . A process of  claim 1 , wherein the hair fibers are heated at a temperature ranging from 120 to 220° C. 
   
   
       19 . A process of  claim 1 , further comprising at least one additional operation chosen from permanent waving, oxidation dyeing, leaching, and straightening.