Strengthened tissue paper products comprising low level of xylan
Est. expiryOct 1, 2022(expired)· nominal 20-yr term from priority
D21H 27/007D21H 17/24D21H 27/30
46
PatentIndex Score
0
Cited by
0
References
0
Claims
Abstract
Disclosed is a tissue paper product comprising one or more plies of a tissue paper; wherein at least one of the plies comprises cellulose and from about 0.005% to about 0.14% by weight based on the weight of cellulose of xylan. Also disclosed is a process for making tissue paper products comprising these ultra low level of xylan.
Claims
exact text as granted — not AI-modified1 . A method for the manufacture of hygienic cellulose paper comprising the steps of:
a) producing a furnish comprising cellulose; b) adding from about 0.005% to about 0.1% by weight, based on the weight of cellulose, of xylan to the furnish, wherein the xylan is a powder or a concentrated liquor; c) forming the furnish into a paper web; d) drying the paper web; and e) creping the dried paper web.
2 . The method of claim 1 wherein the xylan is added to the furnish before forming the furnish into a paper web.
3 . The method of claim 1 wherein the xylan is added to the furnish concurrent with forming the furnish into a paper web.
4 . The method of claim 1 wherein the level of xylan is from about 0.015% to about 0.1% by weight, based on the weight of cellulose.
5 . The method of claim 4 wherein the level of xylan is from about 0.02% to about 0.05% by weight, based on the weight of cellulose.
6 . The method of claim 1 wherein the xylan is a powder having an activity ranging from about 60% to about 80%.
7 . The method of claim 1 further comprising the step of adding from about 0.1 kg/ton (finished paper) to about 2 kg/ton (finished paper) of a cationic charge biasing species to the furnish.Join the waitlist — get patent alerts