US2007176325A1PendingUtilityA1
Polymer transfer apparatus, methods, and composite webs
Assignee: 3M INNOVATIVE PROPERTIES COPriority: Mar 13, 2003Filed: Apr 10, 2007Published: Aug 2, 2007
Est. expiryMar 13, 2023(expired)· nominal 20-yr term from priority
A44B 18/0049B32B 5/04Y10T428/249955B32B 27/12Y10T428/249991B32B 2307/51B32B 3/28B32B 3/02B29L 2031/729B29C 43/222B29C 43/28A44B 18/0061B32B 37/025B32B 2274/00
59
PatentIndex Score
0
Cited by
0
References
0
Claims
Abstract
Composite webs having one or more polymeric structures located on a substrate, methods of manufacturing the composite webs, and systems for manufacturing the composite webs are disclosed. The polymeric structures are formed using thermoplastic compositions deposited into one or more depressions on a forming tool. The forming tool is maintained at a temperature that is below the melt processing temperature of the thermoplastic composition.
Claims
exact text as granted — not AI-modified1 . A method for producing a composite web, the method comprising:
providing a forming tool comprising an exterior surface that comprises one or more depressions formed therein; delivering a molten thermoplastic composition onto the exterior surface of the forming tool; maintaining the exterior surface of the forming tool at a roll temperature that is below a melt processing temperature of the thermoplastic composition; wiping the molten thermoplastic composition on the exterior surface of the forming tool, wherein at least some of the molten thermoplastic composition enters the one or more depressions; transferring the thermoplastic composition in the one or more depressions to a substrate by contacting a first major surface of the substrate to the molten thermoplastic composition in the one or more depressions; separating the substrate and the thermoplastic composition in the one or more depressions from the forming tool after the transferring, wherein a composite web is formed that comprises one or more polymeric structures of the thermoplastic composition located on the first major surface of the substrate, wherein the thermoplastic composition comprises one or more elastomeric polymeric components such that the one or more polymeric structures on the substrate exhibit elastic behavior; and stretching the composite web and the one or more polymeric structures located thereon such that the substrate exhibits permanent elongation after the stretching and such that a portion of the one or more polymeric structures detaches from the first major surface of the substrate.
2 . A method according to claim 1 , wherein a portion of the thermoplastic composition in the one or more depressions that is proximate surfaces of the one or more depressions falls below the melt processing temperature of the thermoplastic composition after the depositing and before the thermoplastic composition in the one or more depressions contacts the first major surface of the substrate.
3 . A method according to claim 1 , wherein a portion of the thermoplastic composition in the one or more depressions that is distal from surfaces of the one or more depressions remains at or above the melt processing temperature at least until the thermoplastic composition in the one or more depressions contacts the first major surface of the substrate.
4 . A method according to claim 1 , wherein a first portion of the thermoplastic composition in the one or more depressions that is proximate surfaces of the one or more depressions falls below the melt processing temperature of the thermoplastic composition after the depositing and before the thermoplastic composition in the one or more depressions contacts the first major surface of the substrate,
and wherein a second portion of the thermoplastic composition in the one or more depressions that is distal from the surfaces of the one or more depressions remains at or above the melt processing temperature of the thermoplastic composition at least until the thermoplastic composition in the one or more depressions contacts the first major surface of the substrate.
5 . A method according to claim 1 , wherein the roll temperature is 20 degrees Celsius or more below a molten thermoplastic composition temperature at which the molten thermoplastic composition is delivered to the exterior surface of the forming tool.
6 . A method according to claim 1 , wherein delivering the molten thermoplastic composition onto the exterior surface of the forming tool comprises extruding the molten thermoplastic composition into an interface between the exterior surface of the forming tool and a doctor blade.
7 . A method according to claim 1 , wherein delivering the molten thermoplastic composition onto the exterior surface of the forming tool comprises extruding the molten thermoplastic composition onto a doctor blade, wherein the molten thermoplastic composition flows down a surface of the doctor blade to an interface between the doctor blade and the exterior surface of the roll.
8 . A method according to claim 1 , wherein the first major surface of the substrate comprises a porous surface, and wherein the transferring further comprises forcing a portion of the first major surface of the substrate against the thermoplastic composition in the one or more depressions, wherein a portion of the thermoplastic composition in at least some depressions of the one or more depressions infiltrates the porous surface.
9 . A method according to claim 8 , wherein the porous surface of the substrate comprises fibers, and further wherein the transferring further comprises encapsulating at least a portion of at least some of the fibers in the thermoplastic composition in the one or more depressions.
10 . A method according to claim 1 , wherein the first major surface of the substrate comprises fibers, and further wherein the transferring further comprises encapsulating at least a portion of at least some of the fibers in the thermoplastic composition by forcing the first major surface of the substrate against the thermoplastic composition in the one or more depressions.
11 . A method according to claim 1 , wherein the substrate comprises polymeric material with a melt processing temperature at or below the melt processing temperature of the thermoplastic composition.
12 . A method according to claim 1 , wherein the wiping leaves some of the molten thermoplastic composition on the exterior surface of the forming tool outside of the one or more depressions.
13 . A method according to claim 1 , wherein depositing the molten thermoplastic composition on the exterior surface of the forming tool comprises depositing two or more different molten thermoplastic compositions on the exterior surface of the forming tool.Join the waitlist — get patent alerts
Track US2007176325A1 — get alerts on status changes and closely related new filings.
We store only your email — no account needed. See our privacy policy.