Composition for improving wrinkle resistance in fabrics, wrinkle-reducing active ingredient as used in such a composition, and cartridge containing such composition
Individually held — no corporate assignee on recordPriority: Aug 21, 2002Filed: Aug 5, 2003Published: May 25, 2006
Est. expiryAug 21, 2022(expired)· nominal 20-yr term from priority
Inventors:Amar Ashok Mavinkurve
D06M 15/693D06M 23/06D06M 23/10D06F 75/22D06M 2200/20D06M 23/02D06M 15/263D06F 75/14
45
PatentIndex Score
0
Cited by
0
References
0
Claims
Abstract
The invention relates to a composition to improve wrinkle resistance in fabrics, comprising: a wrinkle-reducing active ingredient, comprising at least one fusible elastomer and cross-linked particles, and a liquid carrier for carrying the active ingredient. The invention also relates to a wrinkle-reducing active ingredient as used in such a composition and a cartridge for an iron containing such a composition.
Claims
exact text as granted — not AI-modified1 . Composition to improve wrinkle resistance in fabrics, comprising:
a wrinkle-reducing active ingredient, comprising at least one fusible elastomer, and a liquid carrier for carrying the active ingredient, characterized in that the wrinkle-reducing active ingredient further comprises a filler which is at least partly provided with chemically crosslinked particles.
2 . Composition according to claim 1 , characterized in that the filler consists entirely of chemically crosslinked particles.
3 . Composition according to claim 1 , characterized in that the filler is provided with a thermoplast, preferably polymethylmethacrylate (PMMA).
4 . Composition according to claim 1 , characterized in that the content of the active ingredient in the liquid carrier is between 2 and 60% by weight.
5 . Composition according to claim 1 , characterized in that the filler content in the active ingredient is between 5 and 50% by weight, preferably between 10 and 20% by weight.
6 . Composition according to claim 1 , characterized in that the elastomer has a softening temperature between 50 and 150° C. in the presence of water.
7 . Composition according to claim 1 , characterized in that the composition is provided with additives, preferably a surfactant or a perfume.
8 . Wrinkle-reducing active ingredient as used in a composition according to claim 1 .
9 . Cartridge designed for an iron and containing a composition according to claim 1.Join the waitlist — get patent alerts