US2005112308A1PendingUtilityA1
Multilayered plastic container
Est. expiryJun 25, 2022(expired)· nominal 20-yr term from priority
B29C 2949/0715B29C 49/071B29C 2949/3008B29C 2949/0777B29C 2949/3016B29C 2949/302B29C 2949/3042B29C 2949/3012B29C 2949/3028B29C 2949/0773B29C 2949/3032B29C 2949/0819B29C 2949/073B29K 2105/258B29K 2027/18B32B 27/08B65D 81/266B29K 2105/26B29K 2067/00B29K 2023/06B29K 2067/006B29K 2055/02B65D 1/0215B29K 2023/086B32B 2305/70B29B 11/08B29K 2077/00B32B 37/153B29K 2025/00B29K 2081/06B32B 2272/00B29L 2031/7158B29B 11/10B29K 2027/06B29K 2069/00B29K 2023/12B32B 2307/74B29K 2995/0067B29B 11/14Y10T428/1352
52
PatentIndex Score
0
Cited by
0
References
0
Claims
Abstract
A three or more layered plastic container is provided, wherein the innermost first layer is a plastic layer, the intermediate second layer is a plastic layer adjacent the first layer containing an oxygen scavenging material, and the outermost third layer is a plastic layer. The thickness of the innermost layer is in the range of 0.1 to 3 mils and is controlled based on the desired shelf life of the container in the unfilled condition.
Claims
exact text as granted — not AI-modified1 - 12 . (canceled)
13 . The process which comprises:
forming a multilayered plastic container having an upper wall portion, an intermediate sidewall portion and a self-supporting base portion, said portions formed from at least an innermost first layer, an intermediate second layer and an outermost third layer; and wherein said innermost first layer is formed from a plastic material having a thickness of from 0.1 to 3 mils, said intermediate second-layer is formed from a plastic material containing at least one oxygen scavenging material and having a thickness of from 0.1 to 3 mils, and said outermost third layer is formed from a plastic material having a thickness of from 3 to 23 mils.
14 . The process according to claim 13 , including forming the innermost first layer from a plastic material approved for contact with food or beverage products, and controlling the thickness of the innermost first layer in the range of 0.1 to 3 mils based on the desired shelf life of the container in the unfilled condition.
15 . The process according to claim 13 , including the step of forming a blow molded container.
16 . The process according to claim 13 , including forming said container from a multilayered preform, including forming extrusion molded innermost and intermediate layers and an injection molded outermost layer.
17 . The process according to claim 13 , including providing at least 5% of recycled plastic material in the outermost layer.
18 . The process according to claim 13 , including providing that the outermost layer comprises at least 40% by weight of the total weight of the container.
19 . The process according to claim 13 , including providing that the intermediate layer contains a barrier material.
20 . The process according to claim 13 , including providing that at least one layer has differing thicknesses.Join the waitlist — get patent alerts
Track US2005112308A1 — get alerts on status changes and closely related new filings.