US2005089371A1PendingUtilityA1
Method of preparing an asphalt paving material containing recycled plastics
Priority: Oct 24, 2003Filed: May 11, 2004Published: Apr 28, 2005
Est. expiryOct 24, 2023(expired)· nominal 20-yr term from priority
Inventors:Gina Gallant
E01C 19/1004C08L 95/00E01C 19/1031C08L 2207/20E01C 19/1072
16
PatentIndex Score
0
Cited by
0
References
0
Claims
Abstract
A method of forming an asphalt paving material containing recycled plastics. A first step involves forming recycled plastics into plastic particles. A second step involves dry mixing and heating aggregate and sand. A third step involves dry mixing untreated plastic particles with the aggregate and sand, while continuing heating until the mixture of plastic particles, aggregate and sand reaches a temperature range provided in accepted road building specifications for heating aggregate. A fourth step involves adding liquid asphalt to the mixture of plastic particles, aggregate and sand.
Claims
exact text as granted — not AI-modified1 . A method of forming an asphalt paving material containing recycled plastics, comprising the steps of:
forming recycled plastics into plastic particles; dry mixing and heating aggregate and sand; dry mixing untreated plastic particles with the aggregate and sand, while continuing heating until the mixture of plastic particles, aggregate and sand reaches a temperature range provided in accepted road building specifications for heating aggregate; and adding liquid asphalt to the mixture of plastic particles, aggregate and sand.
2 . The method as defined in claim 1 , the plastic particles ranging in size from a powder to one quarter inch granules.
3 . The method as defined in claim 1 , the plastic particles having jagged edges.
4 . The method as defined in claim 1 , the mixture of plastic particles and aggregate being brought within a temperature range of between 280 degrees and 310 degrees fahrenheit.
5 . The method as defined in claim 1 , the plastic particles constituting between one percent and ten percent of by weight of the plastic particles, aggregate and liquid asphalt.
6 . The method as defined in claim 5 , the plastic particles constituting between one percent and four percent by weight.
7 . The method as defined in claim 1 , the recycled plastic being an unclassified mixture of plastics.
8 . The method as defined in claim 1 , the recycled plastic being from Class 2.
9 . A method of forming an asphalt paving material containing recycled plastics, comprising the steps of:
forming recycled plastics into plastic particles ranging in size from a powder to one quarter inch granules; dry mixing and heating aggregate and sand; dry mixing untreated plastic particles with the aggregate and sand, while continuing heating until the mixture of plastic particles, aggregate and sand reaches a temperature range of between 280 degrees and 310 degrees Fahrenheit; and adding liquid asphalt to the mixture of plastic particles, aggregate and sand until the there is between 6 percent and 8 percent liquid asphalt by weight, between 1 percent and 10 percent plastic particles by weight, aggregate and sand.
10 . The method as defined in claim 9 , the plastic particles having jagged edges.
11 . The method as defined in claim 9 , the plastic particles constituting between one percent and four percent by weight.
12 . The method as defined in claim 9 , the recycled plastic being an unclassified mixture of plastics.
13 . The method as defined in claim 9 , the recycled plastic being from Class 2.Join the waitlist — get patent alerts
Track US2005089371A1 — get alerts on status changes and closely related new filings.
We store only your email — no account needed. See our privacy policy.