Total chlorine free bleaching of arundo donax pulp
Abstract
Composite panels and pulp, and paper products of the pulp, are produced from Arundo donax . In the fabrication of the composite panels, Arundo donax is comminuted to a suitable size, combined with a binder, and consolidated into panels that meet standards for construction and/or furniture grade panels. The Arundo donax particulates may be combined with wood particulates to produce a mixed furnish that can be used in the preparation of composite panels. Comminuted Arundo donax is treated, in conventional pulping processes, to produce a high tensile strength pulp that can be used in the production of paper. The pulp has a lighter color than wood pulp, and thereby uses less bleaching chemicals to achieve a desired whiteness. The pulp can be combined with wood pulp to produce a variety of products.
Claims
exact text as granted — not AI-modified1 . A method for forming bleached Arundo donax pulp, comprising:
(a) subjecting a furnish comprising Arundo donax particles to a pulping process to provide Arundo donax pulp; and (b) bleaching the Arundo donax pulp by a total chlorine free process to provide a bleached pulp, wherein bleached pulp has a brightness of at least about 60% ISO.
2 . The method of claim 1 , wherein bleaching comprises the sequence: O(Q)-Eop-P-P-P.
3 . The method of claim 1 , wherein bleaching comprises the sequence: O(Q)-Eop-P-Pp-P.
4 . The method of claim 1 , wherein bleaching comprises the sequence: O-A-P-P-P.
5 . The method of claim 1 , wherein bleaching comprises the sequence: O-Eop-P-Q-P-P.
6 . The method of claim 1 , wherein bleaching comprises the sequence: O-Eop-Q-P-P-P.
7 . The method of claim 1 , wherein bleaching comprises the sequence: O-Q-Eop-P-P-P.
8 . The method of claim 1 , wherein bleaching comprises the sequence: O(Q)-Eop-P-P-P.
9 . Total chlorine free bleached Arundo donax pulp.
10 . The method of claim 1 , wherein the bleached pulp has a brightness of at least about 70% ISO.
11 . The method of claim 1 , wherein the bleached pulp has a brightness of at least about 85% ISO.
12 . A method for forming bleached Arundo donax pulp, comprising:
(a) subjecting a furnish comprising Arundo donax particles to a pulping process to provide Arundo donax pulp, wherein the pulping process comprises cooking the furnish using an H-factor of about 850; and (b) bleaching the Arundo donax pulp by a total chlorine free process to provide a bleached pulp.
13 . The method of claim 12 , wherein the bleached pulp has a brightness of at least about 60% ISO.
14 . The method of claim 12 , wherein the bleached pulp has a brightness of at least about 70% ISO.
15 . The method of claim 12 , wherein the bleached pulp has a brightness of at least about 85% ISO.Join the waitlist — get patent alerts
Track US2005022951A1 — get alerts on status changes and closely related new filings.
We store only your email — no account needed. See our privacy policy.