Fibrous crystal aggregates, preparation method thereof and use thereof
Abstract
A crystal substance formed by precipitating as fibrous aggregates by making a metal aliphatic carboxylate dissolve completely in pure water, stirring, and gradually cooling the resulting solution. A method of preparing the fibrous crystal aggregates. A material for recovering flowing oil and method of recovering flowing oil by using the fibrous crystal aggregates. A material for solidifying liquid hydrocarbon, waste tempura oil and edible oil and method of solidifying liquid hydrocarbon, waste tempura oil and edible oil by using the fibrous crystal aggregates. A method of preparing the solidifying material.
Claims
exact text as granted — not AI-modifiedWhat is claimed is:
1 . A crystal substance, which is formed by precipitating as fibrous aggregates by making a metal aliphatic carboxylate dissolve completely in pure water to give a solution, stirring, and gradually cooling the solution.
2 . A material for recovering oil flowing into rivers, lakes, marshes or the sea, which comprises the fibrous crystal aggregates according to claim 1 .
3 . A crystal substance, which is prepared by precipitating as fibrous aggregates by making a metal aliphatic carboxylate dissolve completely in pure water to give a solution, adding an aqueous solution of an inorganic salt containing the same metal as in the metal aliphatic carboxylate, stirring, and gradually cooling the solution.
4 . A material for recovering oil flowing into rivers, lakes, marshes or the sea, which comprises the fibrous crystal aggregates according to claim 3 .
5 . A method of preparing a fibrous crystal substance, which comprises the steps of: making a metal aliphatic carboxylate dissolve completely in pure water to give a solution; stirring; and gradually cooling the solution, thereby precipitating as fibrous aggregates.
6 . A method of preparing a fibrous crystal substance, which comprises the steps of: making a metal aliphatic carboxylate dissolve completely in pure water to give a solution; adding an aqueous solution of an inorganic salt containing the same metal as in the metal aliphatic carboxylate; stirring; and gradually cooling the solution, thereby precipitating as fibrous aggregates.
7 . A method of solidifying waste tempura oil, which comprises the step of: adding the fibrous crystal aggregates according to claim 1 to waste tempura oil, to solidify the waste tempura oil.
8 . A method of solidifying waste tempura oil, which comprises the step of: adding the fibrous crystal aggregates according to claim 3 to waste tempura oil, to solidify the waste tempura oil.
9 . a method of solidifying edible oil, which comprises the step of: solidifying edible oil, by using the fibrous crystal aggregates according to claim 1 .
10 . A method of solidifying edible oil, which comprises the step of: heating a solidified complex containing solidified edible oil, obtained by the method according to claim 9 , to decompose the solidified complex to regenerate to its original metal aliphatic carboxylate and edible oil.
11 . A method of solidifying edible oil, which comprises the step of: solidifying edible oil, by using the fibrous crystal aggregates according to claim 3 .
12 . A method of solidifying edible oil, which comprises the step of: heating a solidified complex containing solidified edible oil, obtained by the method according to claim 11 , to decompose the solidified complex to regenerate to its original metal aliphatic carboxylate and edible oil.Join the waitlist — get patent alerts
Track US2004265467A1 — get alerts on status changes and closely related new filings.
We store only your email — no account needed. See our privacy policy.