The present invention relates to resin composition with superior antioxidant properties, mechanical strength and insulating properties. A mixture of a thermoplastic resin in pellet or granular form and water is heated under pressure at a subcritical condition of the water to melt the thermoplastic resin, and the melted resin is cooled.
Claims
exact text as granted — not AI-modifiedWhat is claimed is:
1 . A resin composition, wherein a mixture of a thermoplastic resin in pellet or granular form and water is melted using heat and pressure under a subcritical condition of the water, and the melted resin is cooled.
2 . The resin composition of claim 1 , wherein the water is natural unchanged water.
3 . The resin composition, of claim 1 , wherein the water is purified water or distilled water containing antioxidizing substances produced by groups of effective microorganisms.
4 . The resin composition of claim 1 , wherein the water is purified water or distilled water.
5 . The resin composition according to claim 1 , wherein the thermoplastic resin is polyethylene or polypropylene.
6 . The resin composition according to claim 1 , wherein the melted resin is cooled using cold water with impurities removed.
7 . A method for manufacturing a resin composition comprising a first stage wherein a thermoplastic resin in pellet or granular form is mixed and stirred in water, a second stage wherein the mixture is heated under a subcritical condition of the water and the thermoplastic resin is melted, and a third stage wherein the melted resin obtained in the second stage is cooled.
8 . The method for manufacturing a resin composition according to claim 7 , wherein the water is natural unchanged water.
9 . The method for manufacturing a resin composition according to claim 7 , wherein the water is purified water or distilled water containing antioxidizing substances produced by groups of effective microorganisms.
10 . The method for manufacturing a resin composition according to claim 7 , wherein the water is purified water or distilled water.
11 . The method according to claim 7 , wherein the melted resin obtained in the second stage is cooled using cold water with impurities removed.
12 . The method for manufacturing a resin composition according to claim 7 , wherein the thermoplastic resin is polyethylene or polypropylene.
13 . The resin composition of claim 3 , wherein the composition is used to insulate and rustproof electrical wiring.
14 . The resin composition of claim 3 , wherein the composition is used to line pipes so that the pipes remain free of rust.Join the waitlist — get patent alerts